2205双相不锈钢不同厚度层的r值与铁素体织构间的关系
CSTR:
作者:
作者单位:

(1.北京科技大学 冶金工程研究院,北京100083; 2.北京科技大学 材料科学与工程学院,北京100083)

作者简介:

陈雨来(1970—), 男,副研究员

通讯作者:

李静媛, lijy@ustb.edu.cn

中图分类号:

TG142.71

基金项目:

国家自然科学基金(51174026);十二五国家科技支撑计划(2015AA03A502)


Relationship between r value and ferritic texture of 2205 duplex stainless steel sheet in various layers
Author:
Affiliation:

(1.Metallurgical Engineering Research Institute, University of Science and Technology Beijing, Beijing 100083, China; 2.School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China)

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    研究了热轧、冷轧及退火状态下,2205双相不锈钢板各厚度层中铁素体相的织构演变规律,以及其对退火板塑性应变比r值的影响.结果表明,热轧板的表层板表现出明显的{001} <110> 织构,而中间层板由于晶粒转动相对滞后,织构强点集中在(118)[16 -24 1]和(001)[-1-20]取向.这种热轧织构的差异造成冷轧、退火之后,各厚度层的织构和平均塑性应变比rm不相同.冷轧板经1 100 ℃,90 s退火,各厚度层的铁素体相均未形成γ纤维再结晶织构,而形成了(112)[1-10]织构和处于(110)[1-18]~(554)[-2-25]取向间的织构,这与Σ9、Σ3和Σ17b重位点阵有着密切的关系,分别是(001)[1-10](001)[-1-10]和(110)[1-10]冷轧织构的再结晶产物.这类织构使得与轧向成0°的r值明显低于45°及90°的.另外,由于中间层板退火后残留的{001} <110> 取向较少, 因此中间层板的rm高于表层板.

    Abstract:

    The evolution of ferritic texture in various layer of 2205 duplex stainless steel sheet are researched after hot rolled, cold rolled and annealed, and the effects of the textures on plastic strain ratio of the annealed sheet were studied. The results show that the strong {001} <110> texture near surface while concentrated (118)[16 -24 1] and (001)[-1-20] orientation in the center of the hot rolled sheet caused different textures appeared in the surface and center after subsequent cold rolling and annealing processing. It leads to different the average plastic strain ratio in between the surface and center sheet. After annealed at 1100 ℃ for 90 s, (112)[1-10] and (110)[1-18]~(554)[-2-25] recrystallization textures formed from (001)[1-10], (001)[-1-10] and (110)[1-10] cold rolled textures respectively, which is in accordance with Σ9, Σ3 and Σ17b coincidence site lattice relationship. Such annealed textures made that r0 value was significantly lower than r45 and r90 value. Moreover, extremely few {001} <110> orientation was remained in center sheet after annealed, which resulted in a higher average plastic strain ratio in the center sheet.

    参考文献
    相似文献
    引证文献
引用本文

陈雨来,荀晓晨,李静媛.2205双相不锈钢不同厚度层的r值与铁素体织构间的关系[J].哈尔滨工业大学学报,2016,48(11):135. DOI:10.11918/j. issn.0367-6234.2016.11.021

复制
相关视频

分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2016-05-24
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2016-11-09
  • 出版日期:
文章二维码