持续荷载下CFRP-混凝土界面黏结性能试验与分析
CSTR:
作者:
作者单位:

(西南交通大学 土木工程学院, 成都 610031)

作者简介:

马明(1987—),男,博士研究生; 钱永久(1963—),男,教授,博士生导师;

通讯作者:

钱永久,yjqian@sina.com

中图分类号:

U448.22

基金项目:

国家自然科学基金(51508474)


Experiment and performance analysis on bonding behavior of CFRP-concrete interface under sustained load
Author:
Affiliation:

(School of Civil Engineering, Southwest Jiaotong University, Chengdu 610031, China)

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为研究持续荷载对CFRP(碳纤维增强复合材料)-混凝土界面粘结性能的影响,首先通过3组双面剪切试件确定了界面极限剥离荷载Pu,然后进行了4种荷载水平下持载时间分别为5、10、15、30、60、90 d共24组双剪试验.结果表明:经过持续荷载作用,与界面峰值剪应力τmax相应的界面滑移s0有所减小,减小幅度与荷载持续时间和荷载大小无明显相关,荷载作用90 d后,s0降低50%左右;当持续荷载大于0.5Pu时,靠近加载端15 mm范围内的界面峰值剪应力τmax随荷载大小和持载时间的增加而降低,此范围以外τmax未发生明显改变,基于试验数据,给出了持续荷载作用下界面的粘结滑移本构模型,对试件的破坏试验表明,在粘结长度大于有效粘结长度时,持续荷载的作用对界面的极限剥离荷载没有明显影响,但会降低剥离过程中界面首次出现剥离的荷载Pdb,在0.5Pu、0.7Pu、0.9Pu持续作用90 d后,Pdb分别降低了42%、54%、66%.

    Abstract:

    To investigate the effects of sustained load on bonding properties of CFRP (Carbon Fiber Reinforced Polymer)-concrete interface, the ultimate debonding load of interface Pu was determined by three double shear specimens, and twenty-four double shear tests were performed under four load levels and four duration days of 5, 10, 15, 30, 60 and 90 for each load level. Results indicated that the interfacial slip s0 corresponding to the peak interfacial shear stress τmax was reduced under sustained load, but reduction magnitude shows an un-notable correlation with the duration and amplitude of load. The slip s0 reduces by about 50% after the load duration for ninety days. When the load is greater than 0.5Pu, the peak shear stress τmax closed to loading position ranging of 15 mm decrease with the increase of load level and duration, but exhibit un-notable changes in other position. Finally, the bond slip constitutive model of CFRP-concrete interface under sustained load was proposed based on these test data. The failure test showed that there was no significant effect of sustained load on the ultimate debonding load when the bonding length is greater than the effective bonding length, but the peeling load Pdb of interface during the first stripping in the debonding process was reduced due to the sustained load. When the loads of 0.5 Pu, 0.7 Pu, 0.9 Pu last for 90 days, the peeling loads Pdb reduce by 42%, 54%, 66% respectively.

    参考文献
    相似文献
    引证文献
引用本文

马明,徐佰顺,张方,钱永久,李晓斌.持续荷载下CFRP-混凝土界面黏结性能试验与分析[J].哈尔滨工业大学学报,2018,50(3):128. DOI:10.11918/j. issn.0367-6234.201703086

复制
相关视频

分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2017-03-16
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2018-06-14
  • 出版日期:
文章二维码